Propriétés physiques typiques des élastomères communs |
|
|
|
O = Exceptionnel
E =
Excellent
G = Bon
F = Moyen
P = Faible
|
Nom
|
Naturel
|
Uréthane
|
Néoprene
|
Nitrile
|
Butyl
|
EPDM
|
Buna-S
|
Silicone
|
Hypalon
|
Viton®
|
|
Terme ASTM
|
NR/IR
|
AU/EI
|
CR
|
NBR
|
CRIR
|
EPDM
|
SBR
|
SI
|
CSM
|
FKM
|
|
No. pièce Robco
|
140/460
|
Uréthane
|
466/E-60
|
9863
|
930
|
EPP-60/EP-60
|
464
|
960/975
|
HY-60
|
VI-75/VIT-B
|
|
Temp. min.
(F) Cont.
|
-20
|
-10
|
-10
|
-10
|
-10
|
-20
|
0
|
-60
|
-30
|
-10
|
|
Temp. max.
(F) Cont.
|
185
|
185
|
220
|
220
|
220
|
275
|
195
|
460
|
220
|
400
|
|
Abrasion
|
E
|
O
|
G
|
G
|
F
|
G
|
G
|
P
|
G
|
G
|
|
Force Diélectrique
|
E
|
E
|
G
|
P
|
E
|
E
|
E
|
G
|
G
|
G
|
|
Résistance à la flame
|
P
|
F
|
E
|
P
|
P
|
P
|
P
|
G
|
G
|
G
|
|
Vieillisement à la chaleur
(212 deg F)
|
F
|
G
|
G
|
G
|
G
|
E
|
G
|
O
|
E
|
O
|
|
Résistance à l'oxidation
|
G
|
E
|
E
|
G
|
E
|
E
|
F
|
E
|
E
|
O
|
|
Résistance à l'ozone
|
P
|
E
|
E
|
P
|
E
|
O
|
P
|
E
|
O
|
O
|
|
Résistance à la radiation
|
E
|
E
|
G
|
G
|
F
|
O
|
E
|
E
|
G
|
E
|
|
Résistance à la temp.
|
F
|
E
|
G
|
F
|
E
|
E
|
F
|
E
|
E
|
E
|
|
Resistance au déchirement
|
G
|
E
|
G
|
F
|
G
|
G
|
F
|
P
|
F
|
G
|
|
Durée de vie, années (frais, sec, aucun soleil)
|
5
|
8
|
8
|
8
|
8
|
8
|
5
|
20
|
8
|
20+
|
|
Acids concentrés
|
G
|
P
|
G
|
G
|
G
|
E
|
G
|
P
|
E
|
E
|
|
Acids dilue
|
G
|
F
|
G
|
G
|
E
|
E
|
F
|
F
|
E
|
E
|
|
Alkalies concentrés
|
F
|
P
|
P
|
P
|
G
|
E
|
F
|
F
|
G
|
P
|
|
Alkalies dilue
|
G
|
F
|
G
|
G
|
G
|
P
|
F
|
P
|
G
|
P
|
|
Hydrocarbons aliphatiques
|
P
|
G
|
F
|
E
|
P
|
P
|
P
|
P
|
G
|
E
|
|
Hydrocarbons aromatique
|
P
|
P
|
P
|
G
|
P
|
P
|
P
|
P
|
F
|
E
|
|
Huiles– Animal & Végétable
|
F
|
G
|
G
|
E
|
G
|
G
|
F
|
G
|
G
|
E
|
|
Huile et Gasoline
|
P
|
G
|
G
|
E
|
P
|
P
|
P
|
F
|
G
|
E
|
|
| |